GTAW
TG-S12CRS
TIG wire and rod for 9-12%Cr-W-V-Nb steel
| Features: | - Applied for ASTM A335 Gr. P92 and equivalents
- Excellent creep rupture strength
|
|---|
| Classification: | AWS A5.28 ER90S-G |
|---|
| Shielding gas: | Ar |
|---|
| Polarity: | DCEN |
Welding Positions:
Packaging data
| | Spool | Tube |
| φ mm | kg | kg | Length mm | g/piece |
| 1.0 | 10 | - | -
| - |
| 2.0 | - | 5 | 1,000
| 25 |
| 2.4 | - | 5 | 1,000
| 35 |
| Volume mm | 240W, 110H, 230L | 40W, 35H, 1015L |
Composition (wire mass%)
| | Typical | Guarantya |
| C | 0.07 | 0.12 |
| Si | 0.36 | 0.10-0.50 |
| Mn | 0.74 | 0.20-1.00 |
| P | 0.004 | 0.020 |
| S | 0.003 | 0.010 |
| Ni | 0.51 | 0.30-0.80 |
| Cr | 9.92 | 9.50-11.50 |
| Mo | 0.35 | 0.20-0.55 |
| Cu | 0.01 | 0.40 |
|---|
| Nb | 0.04 | 0.01-0.08 |
|---|
| V | 0.21 | 0.10-0.35 |
|---|
| W | 1.45 | 1.00-2.00 |
|---|
| Co | 1.01 | 0.80-1.20 |
|---|
| N | 0.04 | 0.02-0.07 |
| Note: aSingle values are maximium. |
All-weld mechanical properties
| | Typical | Guaranty |
| 0.2%YS (MPa) | 670 | 531min. |
| TS (MPa) | 790 | 621min. |
| EI on 4d (%) | 23 | 17min. |
| IV 0°C (J) | 40 | - |
| PWHT (°Cxh) | 740x8 | 750±15 |