FCAW
DW-50LSR
Flux cored wire
| Features: | - Excellent impact values down to -60°C and down to -50°C in the PWHT condition
- Meets the NACE MR0175 requirements for both chemistry and hardness. The nickel content is normally 1% max.
|
|---|
| Classification: | AWS A5.29 E71T1-GC |
|---|
| Shielding gas: | CO2 |
|---|
| Polarity: | DCEP |
Welding Positions:
Packaging data
| φ mm | Spool |
| 1.2 | 12.5kg | 15kg |
| Volume mm | 300W, 110H, 300L |
Composition (all-weld metal mass %)
| | Typical | Guarantya |
| C | 0.06 | 0.12 |
| Si | 0.29 | 1.00 |
| Mn | 1.34 | 0.50-1.75 |
| P | 0.009 | 0.030 |
| S | 0.007 | 0.030 |
| Ni | 0.88 | 0.70-1.00 |
| Cr | 0.01 | 0.15 |
| Mo | 0.01 | 0.35 |
| V | <0.01 | 0.05 |
| Note: aSingle values are maximium. |
Welding parameters (A)
| φ mm | 1F, 1G, 2F | 2G | 3G uphill, 4G |
| 1.2 | 150-300 | 150-280 | 150-250 |
All-weld mechanical properties
| | Typical | Guaranty |
| 0.2%YS (MPa) | 480 | 425 | 400min. |
| TS (MPa) | 560 | 520 | 483-655 |
| EI on 4d (%) | 31 | 35 | 20min. |
| IV -60°C (J) | 110 | 110 | 27min. |
| PWHT (°Cxh) | AW | 620x1 | AW |
| ABS | 5Y400SA, H5 |
| LR | 5Y40S, H5 |
| DNV | ⅤY40MS (H5) |
| RS | 5Y40SM H5
|